Výsledky vyhledávání
- 1.0534084 - ÚFM 2021 RIV CH eng J - Článek v odborném periodiku
Bürger, D. - Dlouhý, Antonín - Yoshimi, K. - Eggeler, G.
On the stress and temperature dependence of low temperature and high stress shear creep in Ni-base single crystal superalloys.
Materials Science and Engineering A Structural Materials Properties Microstructure and Processing. Roč. 795, SEP (2020), č. článku 139961. ISSN 0921-5093. E-ISSN 1873-4936
Grant CEP: GA MŠMT(CZ) EF16_025/0007304
Institucionální podpora: RVO:68081723
Klíčová slova: steady-state creep * electron-microscopy * power-law * microstructure * deformation * anisotropy * reduction * metals * faults * Ni-base superalloy single crystals * Shear creep deformation * Low-temperature high-stress creep * Stress exponent * Activation energy * Dislocation mechanisms
Obor OECD: Materials engineering
Impakt faktor: 5.234, rok: 2020
Způsob publikování: Open access
https://www.sciencedirect.com/science/article/pii/S0921509320310339?via%3Dihub
Trvalý link: http://hdl.handle.net/11104/0312303 - 2.0497067 - ÚFM 2019 RIV GB eng J - Článek v odborném periodiku
WU, X. - Dlouhý, Antonín - Eggeler, Y. M. - Spiecker, E. - Kostka, A. - Somsen, C. - Eggeler, G.
On the nucleation of planar faults during low temperature and high stress creep of single crystal Ni-base superalloys.
Acta Materialia. Roč. 144, FEB (2018), s. 642-655. ISSN 1359-6454. E-ISSN 1873-2453
Grant CEP: GA ČR(CZ) GA14-22834S
Institucionální podpora: RVO:68081723
Klíčová slova: Ni-base superalloy single crystals * Low temperature and high stress primary creep * Nucleation of planar faults * Gamma channel dislocations
Obor OECD: Materials engineering
Impakt faktor: 7.293, rok: 2018
Trvalý link: http://hdl.handle.net/11104/0289680