Počet záznamů: 1  

Signs of degradation of czech art nouveau mosaic glasses

  1. 1.
    SYSNO ASEP0390201
    Druh ASEPC - Konferenční příspěvek (mezinárodní konf.)
    Zařazení RIVD - Článek ve sborníku
    NázevSigns of degradation of czech art nouveau mosaic glasses
    Tvůrce(i) Rohanová, D. (CZ)
    Švarcová, Silvie (UACH-T) SAI, RID, ORCID
    Hájek, T. (CZ)
    Zdroj.dok.ACTA ARTIS ACADEMICA 2012: KNOWLEDGE AND EXPERIENCE IN THE FINE ART. - PRAHA : Akademie výtvarných umění v Praze, 2012 - ISBN 978-80-87108-33-8
    Rozsah strans. 227-235
    Poč.str.8 s.
    Forma vydáníTištěná - P
    AkceInterdisciplinary Conference of ALMA /4./
    Datum konání21.11.2012-23.11.2012
    Místo konáníPraha
    ZeměCZ - Česká republika
    Typ akceEUR
    Jazyk dok.eng - angličtina
    Země vyd.CZ - Česká republika
    Klíč. slovaglass mosaic ; tesserae ; glass corrosion ; Victor Foerster ; lead glass ; Art Nouveau
    Vědní obor RIVCA - Anorganická chemie
    Institucionální podporaUACH-T - RVO:61388980
    UT WOS000313137700013
    AnotaceAnalyses of Art Nouveau mosaics from the church of St. Simon and Juda in Dolín near Slaný and from Holovousy, both most likely made by the workshop of Viktor Foerster, have shown that the author used the NaO-PbO-SiO 22 glass type and that he used the same glass also for restoration of The Last Judgment mosaic at the Prague Castle in 1890-1910. Despite the fact that lead glasses are more durable than potassium glasses, the material investigations identified corrosion processes on the surface of the glass pieces (tesserae) depending on their composition. Apart from the analyzed mosaic NaO-PbO-SiO2 glasses, we also used ancient sodium glasses (NaO-CaO-SiO2) and 22 potassium glasses (K2O-CaO-SiO2) from archaeological finds in Opava to demonstrate their different chemical durability. We also paid attention to fixation binders used in Art Nouveau mosaics. Inappropriate use of gypsum-containing binders is a significant cause of disintegration of the mosaics. Gypsum and gypsum-lime plasters are very sensitive to humidity. Capillary action of water is a very serious problem that endangers the overall lifespan of any mosaic.
    PracovištěÚstav anorganické chemie
    KontaktJana Kroneislová, krone@iic.cas.cz, Tel.: 311 236 931
    Rok sběru2013