    NázevDevelopment of texture and grain size during extrusion of ZA63 alloy containing stable quasicrystalline i-phase and its effect on tensile and compression strength
    Tvůrce(i) Tesař, Karel (FZU-D) ORCID
    Somekawa, H. (JP)
    Singh, A. (JP)
    Celkový počet autorů3
    Číslo článku156340
    Zdroj.dok.Journal of Alloys and Compounds. - : Elsevier - ISSN 0925-8388
    Roč. 849, Dec (2020), s. 1-11
    Poč.str.11 s.
    Jazyk dok.eng - angličtina
    Země vyd.NL - Nizozemsko
    Klíč. slovametals and alloys ; microstructure ; quasicrystals ; scanning electron microscopy (SEM) ; mechanical properties
    Vědní obor RIVBM - Fyzika pevných látek a magnetismus
    Obor OECDCondensed matter physics (including formerly solid state physics, supercond.)
    Způsob publikováníOmezený přístup
    Institucionální podporaFZU-D - RVO:68378271
    UT WOS000573233800002
    EID SCOPUS85089567020
    DOI10.1016/j.jallcom.2020.156340
    AnotaceWe have focused on dispersion of quasicrystalline i-phase in a Rare Earth-free magnesium alloy Mg6Zn3Al (ZA63). The cast alloy was subjected to a two-step direct extrusion process to study phase (particle) distribution, grain structure, microtexture and related parameters using a host of techniques associated with scanning electron microscopy (SEM) and transmission electron microscopy (TEM), and the resulting mechanical properties. The first extrusion (at 563 K) with a small extrusion ratio of 6.25:1 produced a dispersion of φ phase along the extrusion direction and i-phase decorating the boundaries of grains of size of about 30 μm with a mild basal texture. The second extrusion (at 483 K) with an extrusion ratio of 25:1 reduced the average grain size to 2μm, with comparable yield strength 287.0±4.1 MPa in tension and 299.0 MPa in compression (elongations ~21%).
    PracovištěFyzikální ústav
    KontaktKristina Potocká, potocka@fzu.cz, Tel.: 220 318 579
    Rok sběru2021
    Elektronická adresahttps://doi.org/10.1016/j.jallcom.2020.156340
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.