Structure, processing and performance of ultra-high molecular weight polyethylene (IUPAC Technical Report). Part 1: characterizing molecular weight

  1. 1.
    SYSNO ASEP0532374
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevStructure, processing and performance of ultra-high molecular weight polyethylene (IUPAC Technical Report). Part 1: characterizing molecular weight
    Tvůrce(i) Bucknall, C. (GB)
    Altstädt, V. (DE)
    Auhl, D. (DE)
    Buckley, P. (GB)
    Dijkstra, D. (DE)
    Galeski, A. (PL)
    Gögelein, C. (DE)
    Handge, U. A. (DE)
    He, J. (CN)
    Liu, C.-Y. (CN)
    Michler, G. (DE)
    Piorkowska, E. (PL)
    Šlouf, Miroslav (UMCH-V) RID, ORCID
    Vittorias, I. (CH)
    Wu, J. J. (GB)
    Zdroj.dok.Pure and Applied Chemistry. - : Walter de Gruyter - ISSN 0033-4545
    Roč. 92, č. 9 (2020), s. 1469-1483
    Poč.str.15 s.
    Jazyk dok.eng - angličtina
    Země vyd.DE - Německo
    Klíč. slovahigh temperature creep ; intrinsic viscosity ; IUPAC Polymer Division
    Vědní obor RIVCD - Makromolekulární chemie
    Obor OECDPolymer science
    Způsob publikováníOpen access
    Institucionální podporaUMCH-V - RVO:61389013
    UT WOS000574259400002
    DOI10.1515/pac-2019-0405
    AnotaceThe aim of this project was to study the efficacy of current methods of quality control and quality assurance for ultra-high molecular weight polyethylene (UHMWPE) products, and find improvements where possible. Intrinsic viscosity (IV) tests were performed on three grades of polyethylene with weight average relative molar masses ̅Mw of about 6 × 105, 5.0 × 106 and 9.0 × 106. Results from three laboratories showed substantial scatter, probably because different methods were used to make and test solutions. Tensile tests were carried out to 600 % extension at 150 °C under both constant applied load and constant Hencky strain rate, on compression mouldings made by a leading manufacturer of ultra-high molecular weight polyethylene. They gave low values of ̅Mw, suggesting incomplete entanglement at ‘grain boundaries’ between powder particles. Results from conventional melt-rheology tests are presented, and their relevance to quality control and assurance is discussed. Attempts to calculate molecular weights from these data met with limited success because of extended relaxation times. Suggestions are made for improving international standards for IV testing of UHMWPE, by investigating the various factors that can cause significant errors, and by introducing methods for checking the homogeneity (and hence validity) of the solutions tested. Part 2 addresses characterization of crystallinity and structure. Part 3 covers mechanical properties, and Part 4 focuses on the sporadic crack propagation behaviour exhibited by all three grades of UHMWPE in fatigue tests on 10 mm thick compact tension specimens.
    PracovištěÚstav makromolekulární chemie
    KontaktEva Čechová, cechova@imc.cas.cz ; Tel.: 296 809 358
    Rok sběru2021
    Elektronická adresahttps://www.degruyter.com/view/journals/pac/92/9/article-p1469.xml?tab_body=abstract
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.