Počet záznamů: 1  

Laser performances of diode pumped Yb:Lu.sub.2./sub.O.sub.3./sub. transparent ceramic at cryogenic temperatures

  1. 1.
    SYSNO ASEP0518033
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevLaser performances of diode pumped Yb:Lu2O3 transparent ceramic at cryogenic temperatures
    Tvůrce(i) David, Samuel Paul (FZU-D) ORCID
    Jambunathan, Venkatesan (FZU-D)
    Yue, Fangxin (FZU-D) ORCID
    Le Garrec, Bruno (FZU-D)
    Lucianetti, Antonio (FZU-D) RID, ORCID
    Mocek, Tomáš (FZU-D) RID, ORCID, SAI
    Celkový počet autorů6
    Zdroj.dok.Optical Materials Express. - : Optical Society of America - ISSN 2159-3930
    Roč. 9, č. 12 (2019), s. 4669-4676
    Poč.str.8 s.
    Jazyk dok.eng - angličtina
    Země vyd.US - Spojené státy americké
    Klíč. slovacryogenic temperature ; Yb:Lu2O3
    Vědní obor RIVBH - Optika, masery a lasery
    Obor OECDOptics (including laser optics and quantum optics)
    CEPEF15_006/0000674 GA MŠMT - Ministerstvo školství, mládeže a tělovýchovy
    LO1602 GA MŠMT - Ministerstvo školství, mládeže a tělovýchovy
    Způsob publikováníOmezený přístup
    Institucionální podporaFZU-D - RVO:68378271
    UT WOS000499348700018
    EID SCOPUS85077146207
    DOI10.1364/OME.9.004669
    AnotaceTwo different fiber coupled diode pump sources, one emitting around 975.7 nm volume Bragg grating (VBG) stabilized and another around 940 nm were used for comparison. Under the pump at 975.7 nm and 100 K cryogenic temperature, the laser yielded CW output power of 11.24 W for 20.3 W incident pump power, corresponding to an overall optical-to optical efficiency of 55%, the slope efficiency was 59%. For operation at room temperature, the output power was limited to 4.44 W whereas the slope efficiency was 27.5%. Optimum operation under 940 nm pump was obtained at 80 K. Under 940 nm pumping, Yb:Lu2O3 medium generated a CW output power of 3 W for 20 W, the slope efficiency was around 17%. The passive Q-switch operation was investigated with Cr4+:YAG saturable absorber (SA) crystal, employing the pump at 975.7 nm. Laser pulses with an energy of 0.35 mJ and a pulse duration of 116 ns at 26.1 kHz repetition rate were recorded with a Cr4+:YAG SA having 85% initial transmission.
    PracovištěFyzikální ústav
    KontaktKristina Potocká, potocka@fzu.cz, Tel.: 220 318 579
    Rok sběru2020
    Elektronická adresahttps://doi.org/10.1364/ome.9.004669
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.