Elastic and anelastic behavior of TBCs sprayed at high-deposition rates

  1. 1.
    SYSNO ASEP0456064
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevElastic and anelastic behavior of TBCs sprayed at high-deposition rates
    Tvůrce(i) Valarezo, A. (US)
    Dwivedi, G. (US)
    Sampath, S. (US)
    Mušálek, Radek (UFP-V) RID, ORCID
    Matějíček, Jiří (UFP-V) RID, ORCID
    Zdroj.dok.Journal of Thermal Spray Technology. - : Springer - ISSN 1059-9630
    Roč. 24, 1-2 (2015), s. 160-167
    Poč.str.8 s.
    Forma vydáníTištěná - P
    Jazyk dok.eng - angličtina
    Země vyd.US - Spojené státy americké
    Klíč. slovadense vertically cracked coating ; elastic modulus ; in-situ monitoring ; mechanical properties ; quenching stress ; thermal barrier coatings (TBCs) ; triplex system
    Vědní obor RIVJK - Koroze a povrchové úpravy materiálů
    CEPME 901 GA MŠMT - Ministerstvo školství, mládeže a tělovýchovy
    GPP108/12/P552 GA ČR - Grantová agentura ČR
    Institucionální podporaUFP-V - RVO:61389021
    UT WOS000347416800020
    EID SCOPUS84925496137
    DOI10.1007/s11666-014-0154-6
    AnotaceCoatings sprayed at high-deposition rates often result in stiff, dense, and highly stressed coatings. The high deposition temperature at which the coatings are formed is responsible for these characteristics. In this paper, TBCs were sprayed at high-deposition rates, increasing the tensile quenching stresses beyond the threshold of crack opening during spraying. Dense structures were observed within a pass, in the presence of micro and macro defects specifically horizontal cracks within interpasses and vertical segmentation cracks. Mechanical properties, mainly the elastic and anelastic behavior of TBCs were significantly affected by the strain accommodation and friction occurring within intersplats and interpass interfaces. The strain tolerance obtained in as-sprayed conditions decreased as the microstructure and defects sintered during high-temperature heat cycles. The non-linearity degree decreased while the elastic modulus of the various coatings increased to a maximum value.
    PracovištěÚstav fyziky plazmatu
    KontaktVladimíra Kebza, kebza@ipp.cas.cz, Tel.: 266 052 975
    Rok sběru2016
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.