Počet záznamů: 1  

Exploitation of modern physical techniques in characterization of accelerated weathering processes in commodity polymers; ESRI, ATR FTIR and diffuse transmittance measurements

  1. 1.
    SYSNO ASEP0364739
    Druh ASEPC - Konferenční příspěvek (mezinárodní konf.)
    Zařazení RIVD - Článek ve sborníku
    NázevExploitation of modern physical techniques in characterization of accelerated weathering processes in commodity polymers; ESRI, ATR FTIR and diffuse transmittance measurements
    Tvůrce(i) Pilař, Jan (UMCH-V) RID, ORCID
    Šeděnková, Ivana (UMCH-V) RID
    Pfleger, Jiří (UMCH-V) RID
    Michálková, Danuše (UMCH-V)
    Zdroj.dok.Natural and Artificial Ageing of Polymers, Publication No.15. - Pfinztal : Confederation of European Environmental Engineering Societies (CEEES) - Gesellschaft für Umweltsimulation GUS, 2011 / Reichert T. - ISBN 978-3-9813136-2-8
    Rozsah strans. 359-369
    Poč.str.11 s.
    AkceEuropean Weathering Symposium /5./
    Datum konání21.09.2011-23.09.2011
    Místo konáníLisbon
    ZeměPT - Portugalsko
    Typ akceWRD
    Jazyk dok.eng - angličtina
    Země vyd.DE - Německo
    Klíč. slovacommodity polymers ; photodegradation ; diffuse transmittance
    Vědní obor RIVCD - Makromolekulární chemie
    CEPIAA400500804 GA AV ČR - Akademie věd
    CEZAV0Z40500505 - UMCH-V (2005-2011)
    AnotaceWeathering of polymers comprises a large number of photooxidation processes triggered by environmental factors. It accounts for heterogeneous photodegradation that has negative impact on material properties of polymers. The degradation can be minimized by application of stabilizers, hindered amine stabilizers (HAS) in particular. We applied modern physical techniques that are able to bring unique information on the heterogeneity of the degradation process. Development of concentration profiles of nitroxides inside polymer plaques and concentrations of oxidation products on the surfaces and inside the plaques were determined by ESRI and by ATR FTIR, respectively. Diffuse optical transmission of the plaques was determined using spectrophotometer equipped with an integration sphere. Data determined in four commodity carbon chain polymers PP, PE, PS and Topas® stabilized with secondary HAS Tinuvin® 770 and with Tinuvin® NOR 123 are compared.
    PracovištěÚstav makromolekulární chemie
    KontaktEva Čechová, cechova@imc.cas.cz ; Tel.: 296 809 358
    Rok sběru2012
    Elektronická adresahttp://www.weathering-symposium.org/books/books.htm
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.