Počet záznamů: 1  

Improvement of surface integrity of Nimonic C 263 super alloy produced by WEDM through various post-processing techniques

  1. SYS0475860
    LBL
      
    01000a^^22220027750^450
    005
      
    20240111140942.3
    014
      
    $a 000412903700038 $2 WOS
    017
      
    $a 10.1007/s00170-017-9993-x $2 DOI
    100
      
    $a 20170629d m y slo 03 ba
    101
      
    $a eng $d eng
    102
      
    $a DE
    200
    1-
    $a Improvement of surface integrity of Nimonic C 263 super alloy produced by WEDM through various post-processing techniques
    215
      
    $a 11 s. $c E
    463
    -1
    $1 001 cav_un_epca*0253343 $1 011 $a 0268-3768 $e 1433-3015 $1 200 1 $a International Journal of Advanced Manufacturing Technology $v Roč. 93, 1-4 (2017), s. 433-443 $1 210 $c Springer
    610
      
    $a surface integrity
    610
      
    $a wire-EDM
    610
      
    $a Nimonic C-263
    610
      
    $a multi-cut
    610
      
    $a recast layer
    700
    -1
    $3 cav_un_auth*0330768 $4 070 $a Mandal $b A. $y IN
    701
    -1
    $3 cav_un_auth*0331376 $4 070 $a Dixit $b A. R. $y IN
    701
    -1
    $3 cav_un_auth*0301163 $4 070 $a Chattopadhyaya $b S. $y IN
    701
    -1
    $3 cav_un_auth*0347417 $4 070 $a Paramanik $b A. $y AU
    701
    -1
    $3 cav_un_auth*0295988 $i Oddělení dezintegrace materiálů $j Department of material disintegration $w Material Disintegration $4 070 $a Hloch $b Sergej $p UGN-S $y CZ $T Ústav geoniky AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0347418 $4 070 $a Królczyk $b G. $y PL
    856
      
    $9 RIV $q textový soubor $u https://link.springer.com/article/10.1007/s00170-017-9993-x
Počet záznamů: 1  