Correlation between microstructure and creep performace of martensitic/austenitic transition weldment in dependence of its post-weld heat treatment

  1. SYS0428406
    LBL
      
    01811^^^^^2200361^^^450
    005
      
    20240103204246.8
    014
      
    $a 000334020000012 $2 WOS
    017
    70
    $a 10.1016/j.engfailanal.2014.02.018 $2 DOI
    100
      
    $a 20141127d m y slo 03 ba
    101
    0-
    $a eng $d eng
    102
      
    $a GB
    200
    1-
    $a Correlation between microstructure and creep performace of martensitic/austenitic transition weldment in dependence of its post-weld heat treatment
    215
      
    $a 12 s.
    463
    -1
    $1 001 cav_un_epca*0252819 $1 011 $a 1350-6307 $e 1873-1961 $1 200 1 $a Engineering Failure Analysis $v Roč. 40, MAY (2014), s. 141-152 $1 210 $c Elsevier
    610
    0-
    $a transition weldment: T92/TP316H
    610
    0-
    $a post-weld heat treatment
    610
    0-
    $a microstructure
    700
    -1
    $3 cav_un_auth*0280589 $a Falat $b L. $y SK $4 070
    701
    -1
    $3 cav_un_auth*0297574 $a Čiripová $b L. $y SK $4 070
    701
    -1
    $3 cav_un_auth*0280590 $a Kepič $b J. $y SK $4 070
    701
    -1
    $3 cav_un_auth*0101245 $a Buršík $b Jiří $i Struktura fází $j Structure of Phases $p UFM-A $w Structure of Phases and Thermodynamics Group $4 070 $T Ústav fyziky materiálů AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0303370 $a Podstranská $b Ivana $i Struktura fází $j Structure of Phases $p UFM-A $4 070 $T Ústav fyziky materiálů AV ČR, v. v. i.
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.