    NázevTomographic investigation of the fracture toughness of the quasi-brittle specimens subjected to four-point bending test
    Tvůrce(i) Vavřík, Daniel (UTAM-F) RID, SAI, ORCID
    Beneš, Pavel (UTAM-F) RID, SAI
    Fíla, Tomáš (UTAM-F) RID, SAI, ORCID
    Koudelka_ml., Petr (UTAM-F) RID, SAI, ORCID
    Kumpová, Ivana (UTAM-F) RID, SAI, ORCID
    Kytýř, Daniel (UTAM-F) SAI, RID, ORCID
    Vopálenský, Michal (UTAM-F) RID, ORCID, SAI
    Vavro, Martin (UGN-S) RID, ORCID
    Vavro, Leona (UGN-S) RID
    Celkový počet autorů9
    Zdroj.dok.Procedia Structural Integrity, ECF - Loading and Environmental Effects on Structural Integrity, 13. - Amsterdam : Elsevier, 2018 / Sedmak A. ; Radakovic Z. ; Rakin M. - ISSN 2452-3216
    Rozsah strans. 1967-1970
    Poč.str.4 s.
    Forma vydáníTištěná - P
    AkceEuropean Conference on Fracture /22./
    Datum konání26.08.2018 - 31.08.2018
    Místo konáníBelgrade
    ZeměRS - Srbsko
    Typ akceWRD
    Jazyk dok.eng - angličtina
    Země vyd.NL - Nizozemsko
    Klíč. slovafracture process zone ; crack path ; quasi-brittle material ; X-Ray computed tomography ; four-point bending test
    Vědní obor RIVJJ - Ostatní materiály
    Obor OECDApplied mechanics
    Vědní obor RIV – spolupráceÚstav geoniky - Ostatní materiály
    CEPEF16_019/0000766 GA MŠMT - Ministerstvo školství, mládeže a tělovýchovy
    Institucionální podporaUTAM-F - RVO:68378297 ; UGN-S - RVO:68145535
    UT WOS000459860900321
    EID SCOPUS85064710991
    DOI https://doi.org/10.1016/j.prostr.2018.12.263
    AnotaceIt is well known that detailed investigation of fracture mechanics of the quasi-brittle materials is rather complicated task as standard loading devices do not allow to interrupt loading test after reaching maximal loading force. The reason is that the point of maximal loading force is followed by the evolution of the fracture processes, due to elastic energy stored in the loading device itself. This fundamental obstacle was overcome in this work thanks to a newly developed compact four-point bending device. We show that shape of the crack can be evaluated on the basis of the so called differential tomography, which compares reference and actual states of the loaded specimen. Similarly, it is possible to evaluate displacement and strain fields by analyzing the series of loading states using the digital image correlation tools. Using such a methodology, local fracture toughness KIc is calculated thanks to information about of the crack path and evaluated CTOD parameter.
    PracovištěÚstav teoretické a aplikované mechaniky
    KontaktKulawiecová Kateřina, kulawiecova@itam.cas.cz, Tel.: 225 443 285
    Rok sběru2019
    Elektronická adresahttps://doi.org/10.1016/j.prostr.2018.12.263
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.