Optimization of laboratory hot rolling of brittle Fe-40at.%Al-Zr-B aluminide
- 1.0454901 - FZÚ 2016 RIV PL eng J - Článek v odborném periodiku
Schindler, I. - Hadasik, E. - Kopeček, Jaromír - Kawulok, P. - Fabík, R. - Opěla, P. - Rusz, S. - Kawulok, R. - Jabłońska, M.
Optimization of laboratory hot rolling of brittle Fe-40at.%Al-Zr-B aluminide.
Archives of Metallurgy and Materials. Roč. 60, č. 3 (2015), s. 1693-1701. ISSN 1733-3490. E-ISSN 2300-1909
Grant CEP: GA ČR(CZ) GAP107/10/0438
Institucionální podpora: RVO:68378271
Klíčová slova: iron aluminides * EBSD * textures * modelling
Kód oboru RIV: JG - Hutnictví, kovové materiály
Impakt faktor: 1.090, rok: 2014
Use of the protective steel capsules enabled to manage the laboratory hot flat rolling of the extremely brittle as-cast aluminide Fe-40at.%Al-Zr-B with the total height reduction of almost 70 %. The hot rolling parameters were optimized to obtain the best combination of deformation temperature (from 1160°C up to 1240°C) and rolling speed (from 0.14 m·s-1 to 0.53 m·s-1). The resistance against cracking and refinement of the highly heterogeneous cast microstructure were themain criteria. Both experiments and mathematical simulations based on FEM demonstrated that it is not possible to exploitenhanced plasticity of the investigated alloy at low strain rates in the hotrolling process.