Počet záznamů: 1  

Laminated alumina/zirconia ceramic composites prepared by electrophoretic

  1. 1.
    SYSNO ASEP0385457
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevLaminated alumina/zirconia ceramic composites prepared by electrophoretic
    Tvůrce(i) Hadraba, Hynek (UFM-A) RID, ORCID
    Drdlík, D. (CZ)
    Chlup, Zdeněk (UFM-A) RID, ORCID
    Maca, K. (CZ)
    Dlouhý, Ivo (UFM-A) RID, ORCID
    Cihlář, J. (CZ)
    Celkový počet autorů6
    Zdroj.dok.Journal of the European Ceramic Society. - : Elsevier - ISSN 0955-2219
    Roč. 32, č. 9 (2012), s. 2053-2056
    Poč.str.4 s.
    AkceEngineering Ceramics 2011 - from Materials to Components
    Datum konání09.05.2011-12.05.2011
    Místo konáníSmolenice
    ZeměSK - Slovensko
    Typ akceWRD
    Jazyk dok.eng - angličtina
    Země vyd.GB - Velká Británie
    Klíč. slovaelectrophoretic deposition ; composites ; hardness ; Al2O3 ; ZrO2
    Vědní obor RIVJH - Keramika, žáruvzdorné materiály a skla
    CEPGAP108/11/1644 GA ČR - Grantová agentura ČR
    Institucionální podporaUFM-A - RVO:68081723
    CEZAV0Z20410507 - UFM-A (2005-2011)
    UT WOS000303626200028
    DOI https://doi.org/10.1016/j.jeurceramsoc.2011.09.004
    AnotaceThe electrophoretic deposition of alumina and zirconia powders from isopropanolic suspension in the presence of monochloracetic acid was studied in the constant-current regime. The different levels of electric current during deposition from 250 µA to 48 mA were used. The green density of the deposit depends on the current density and then on the particle velocity during deposition, reaching values from 58% to 61% according to the electric current used. It was found that the lower the green density of the green deposit, the larger the pores. The low green density led to low final fired density and subsequently to the low Vickers hardness HV5 ranging from 2000 to 1650 depending on electric current used. Based on these findings microlaminates having various thickness ratios to achieve different residual stress levels were prepared consisting of alternating layers of alumina and zirconia.
    PracovištěÚstav fyziky materiálu
    KontaktYvonna Šrámková, sramkova@ipm.cz, Tel.: 532 290 485
    Rok sběru2013
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.