Effect of halloysite nanotubes on the thermal degradation behaviour of poly(.epsilon.-caprolactone)/poly(lactic acid) microfibrillar composites

  1. SYS0473691
    LBL
      
    01000a^^22220027750^450
    005
      
    20240103213935.0
    014
      
    $a 85016322695 $2 SCOPUS
    014
      
    $a 000403122100023 $2 WOS
    017
      
    $a 10.1016/j.polymertesting.2017.03.027 $2 DOI
    100
      
    $a 20170331d m y slo 03 ba
    101
      
    $a eng
    102
      
    $a GB
    200
    1-
    $a Effect of halloysite nanotubes on the thermal degradation behaviour of poly(.epsilon.-caprolactone)/poly(lactic acid) microfibrillar composites
    215
      
    $a 7 s.
    463
    -1
    $1 001 cav_un_epca*0257491 $1 011 $a 0142-9418 $e 1873-2348 $1 200 1 $a Polymer Testing $v Roč. 60, July (2017), s. 166-172 $1 210 $c Elsevier
    610
      
    $a poly(lactic acid)
    610
      
    $a poly(epsilon-caprolactone)
    610
      
    $a halloysite nanotubes
    700
    -1
    $3 cav_un_auth*0345479 $4 070 $a Luyt $b A. S. $y QA $z K
    701
    -1
    $3 cav_un_auth*0103061 $i Polymerní materiály a technologie $j Polymer Materials and Technologies $k MATER $l MATER $w Polymer materials $4 070 $a Kelnar $b Ivan $p UMCH-V $T Ústav makromolekulární chemie AV ČR, v. v. i.