Boronized stainless steel with zirconia coatings

  1. 1.
    SYSNO ASEP0456147
    Druh ASEPC - Konferenční příspěvek (mezinárodní konf.)
    Zařazení RIVD - Článek ve sborníku
    NázevBoronized stainless steel with zirconia coatings
    Tvůrce(i) Brožek, Vlastimil (UFP-V) RID
    Kolísko, J. (CZ)
    Kubatík, Tomáš František (UFP-V)
    Mastný, L. (CZ)
    Pokorný, P. (CZ)
    Tej, P. (CZ)
    Zdroj.dok.METAL 2015: 24th International Conference on Metallurgy and Materials, Conference Proceedings. - Ostrava : TANGER Ltd, 2015 - ISBN 978-80-87294-62-8
    Rozsah strans. 1069-1074
    Poč.str.6 s.
    Forma vydáníTištěná - P
    AkceMETAL 2015. International Conference on Metallurgy and Materials /24./
    Datum konání03.06.2015-05.06.2015
    Místo konáníBrno
    ZeměCZ - Česká republika
    Typ akceWRD
    Jazyk dok.eng - angličtina
    Země vyd.CZ - Česká republika
    Klíč. slovaBoronised steel ; plasma spraying ; ceramic coatings ; bond strength ; zirkonia coatings
    Vědní obor RIVJH - Keramika, žáruvzdorné materiály a skla
    Institucionální podporaUFP-V - RVO:61389021
    UT WOS000374706100172
    AnotaceConditions of boronizing are described using a reactive diffusion method of boron from boron carbide and lanthanum hexaboride so that the formation of Fe2B is preferred to FeB which is more brittle and whose structure does not satisfy the conditions for perfect adhesion of modified zirconia ceramics. Perfectly rigid adhesive connection of needle-like embedded interlayers Fe2B in steel AISI 303 prepared by reactive diffusion of a boronizing medium without activators at 1000 ° C and exposure of 2-4 hours has the value of 20 - 24 MPa at the Pinn-off test.Ceramic coatings from Al2O3-ZrO2 ceramics formed on those interlayers have the value of bond strength up to 14 - 20 MPa.Thermal cycling between 100°C - 600 °C confirmed good adhesion of coatings with the underlying steel.During thermal cycling at elevated temperatures (600-1000 °C) there occurs a statistically significant number of faults in cohesion and mechanical destruction of the coatings. One of the reasons are secondary changes
    PracovištěÚstav fyziky plazmatu
    KontaktVladimíra Kebza, kebza@ipp.cas.cz, Tel.: 266 052 975
    Rok sběru2016
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.