Porous hybrid poly(N-isopropylacrylamide) hydrogels with very fast volume response to temperature and pH

  1. 1.
    SYSNO ASEP0508103
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevPorous hybrid poly(N-isopropylacrylamide) hydrogels with very fast volume response to temperature and pH
    Tvůrce(i) Strachota, Beata (UMCH-V) RID
    Oleksyuk, Khrystyna (UMCH-V)
    Strachota, Adam (UMCH-V) RID, ORCID
    Šlouf, Miroslav (UMCH-V) RID, ORCID
    Číslo článku109213
    Zdroj.dok.European Polymer Journal. - : Elsevier - ISSN 0014-3057
    Roč. 120, November (2019), s. 1-14
    Poč.str.14 s.
    Jazyk dok.eng - angličtina
    Země vyd.GB - Velká Británie
    Klíč. slovapolymeric hydrogels ; smart materials ; nanocomposites
    Vědní obor RIVCD - Makromolekulární chemie
    Obor OECDPolymer science
    CEPGA19-04925S GA ČR - Grantová agentura ČR
    Způsob publikováníOmezený přístup
    Institucionální podporaUMCH-V - RVO:61389013
    UT WOS000498309000005
    EID SCOPUS85071879458
    DOI10.1016/j.eurpolymj.2019.109213
    AnotaceSuper-porous hydrogels were prepared, which are able of fast to ultra-fast volume response to temperature and to pH, and thus show a promise as soft actuators. The hydrogels are based on the poly(N-isopropylacrylamide) (PNIPAm)/silica nanocomposite, in which the filler strongly raises the modulus and also stabilizes the pore walls against collapse during deswelling. The well-interconnected sub-millimetre-sized porosity was generated via solvent freezing during synthesis. The gels morphology makes possible both ultra-fast deswelling and re-swelling (5.5 s for 70% in both directions, in response to T). This work focused on introducing pH-responsiveness into the gels. To this end, 1–10 mol% of sodium methacrylate (SMA) were incorporated as co-monomer. Distinct pH-responsiveness was achieved already at 1 mol% of SMA. Increase of SMA content markedly expands the temperature range of the pH-responsiveness and raises its amplitude. At the same time the increase of SMA content reduces the amplitude of the T-responsiveness, which is only moderate at 10 mol% SMA. The rate of pH-response was found to be always slower than in case of the T-response: 75 s are needed for 70% of de-swelling, and 90 min for 70% of re-swelling. The vast difference in the rates of pH- and T- response can be explained by different mechanisms of stimulus propagation (momentum transfer for T, vs. diffusion for pH) and by the mechanical effect of a contracting stiff and porous surface layer (much faster pH-deswelling than re-swelling). More generally, in case of the pH-stimulus, the mechanistic limits of its propagation in ‘simple’ porous gels become evident.
    PracovištěÚstav makromolekulární chemie
    KontaktEva Čechová, cechova@imc.cas.cz ; Tel.: 296 809 358
    Rok sběru2020
    Elektronická adresahttps://www.sciencedirect.com/science/article/pii/S0014305719313965?via%3Dihub
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.