Počet záznamů: 1  

Recycling of waste poly(ethylene terephthalate) with castor oil using microwave heating

  1. 1.
    SYSNO ASEP0397261
    Druh ASEPJ - Článek v odborném periodiku
    Zařazení RIVJ - Článek v odborném periodiku
    Poddruh JČlánek ve WOS
    NázevRecycling of waste poly(ethylene terephthalate) with castor oil using microwave heating
    Tvůrce(i) Beneš, Hynek (UMCH-V) RID, ORCID
    Slabá, J. (CZ)
    Walterová, Zuzana (UMCH-V)
    Rais, David (UMCH-V) RID
    Zdroj.dok.Polymer Degradation and Stability. - : Elsevier - ISSN 0141-3910
    Roč. 98, č. 11 (2013), s. 2232-2243
    Poč.str.12 s.
    Jazyk dok.eng - angličtina
    Země vyd.NL - Nizozemsko
    Klíč. slovapoly(ethylene terephthalate) ; castor oil ; chemical recycling
    Vědní obor RIVCD - Makromolekulární chemie
    CEP2A-2TP1/135 GA MPO - Ministerstvo průmyslu a obchodu
    Institucionální podporaUMCH-V - RVO:61389013
    UT WOS000327908800016
    DOI10.1016/j.polymdegradstab.2013.08.019
    AnotaceThe chemical recycling of waste poly(ethylene terephthalate) (PET) using castor oil (CO) as a reagent is reported. CO presents a renewable alternative to petrochemical based reagents, e.g. glycols, and enables also substantial modification of final physico-chemical properties of a received product. Advantageously, microwave irradiation was used to accelerate the depolymerization of PET. A composition of obtained product was strongly influenced by the reaction temperature. When the decomposition of PET was performed at temperature higher than 240 °C, then a significant extent of side products based on PET oligomers and transesterified CO was observed due to dehydration and hydrolysis of CO. Contrary to that, PET decomposition took place at slow rate below 230 °C and the optimal reaction temperature lies in the relatively narrow interval from 230 °C to 240 °C. The product prepared in the optimal temperature range did not contain any high molecular weight PET oligomers. MALDI-TOF mass spectrometry enabled to identify the structures included in the obtained polyol product. The maximum number of six repeating monomeric unit of PET was found in the product, which confirmed practically the complete depolymerization of PET chain and good reactivity of the acylester hydroxyl groups of CO.
    PracovištěÚstav makromolekulární chemie
    KontaktEva Čechová, cechova@imc.cas.cz ; Tel.: 296 809 358
    Rok sběru2014
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.