Improvement of hemocompatibility of gamma-Fe2O3 nanoparticles via their covering with complex poly(N,N-dimethylacrylamide) and SiO2 shell

  1. 1.
    0579496 - ÚMCH 2025 RIV DE eng J - Článek v odborném periodiku
    Paryzhak, S. - Dumych, T. - Zasońska, Beata Anna - Svoboda, Jan - Klyuchivska, O. - Skorokhyd, N. - Kozak, Y. - Horák, Daniel - Stoika, R.
    Improvement of hemocompatibility of gamma-Fe2O3 nanoparticles via their covering with complex poly(N,N-dimethylacrylamide) and SiO2 shell.
    Applied Nanoscience. Roč. 13, č. 12 (2023), s. 7399-7412. ISSN 2190-5509. E-ISSN 2190-5517
    Grant CEP: GA ČR(CZ) GC20-02177J
    Institucionální podpora: RVO:61389013
    Klíčová slova: maghemite * nanoparticles * poly(N,N-dimethylacrylamide)
    Obor OECD: Polymer science
    Impakt faktor: 3.869, rok: 2021
    Způsob publikování: Omezený přístup
    https://link.springer.com/article/10.1007/s13204-023-02905-3

    The biocompatibility of NPs to blood cells is a key issue when these NPs are planned for intravenous application because of potential contact with blood cells and proteins. In this work, γ-Fe2O3 NPs (~ 9 nm) and their poly(N,N-dimethylacrylamide) (PDMA) and SiO2-coated derivatives (γ-Fe2O3@PDMA and γ-Fe2O3@SiO2, respectively) were investigated. It was detected that both PDMA and SiO2 coatings decreased NPs’ aggregation in the buffer solutions, as well as in cell culture medium. Neither neat γ-Fe2O3 NPs nor their coated derivatives possessed hemolytic activity toward red blood cells. There was no significant loss of body weight observed after the intravenous injection to laboratory mice. The immune response to the injected NPs was assessed by the ELISA measuring. No antibodies of the IgM class were detected, which suggests lack of acute inflammation. On the 35th day of the experiment, there was a rise in the content of the anti-OVA IgG noticed in all three types of the NPs, however this rise was lower compared to that induced by the positive control. The injected NPs were found to be spread and settled in the pouch cavity, and none of the tested NPs caused vascular damage or distinct signs of inflammation. Summarizing, γ-Fe2O3 NPs coated with the PDMA or SiO2 manifested good compatibility with blood cells in in vitro and in vivo investigations.