    High temperature spherical nano-indentation of graphite crystals.
    Carbon. Roč. 191, MAY (2022), s. 236-242. ISSN 0008-6223. E-ISSN 1873-3891
    Institucionální podpora: RVO:68081723
    Klíčová slova: in-situ measurement * nuclear graphite * elastic-constants * youngs modulus * mechanical-properties * nonlinear elasticity * basal-plane * kink bands * nanoindentations * composites * Graphite * Nanoindentation * Kink band * High temperature
    Obor OECD: Materials engineering
    Impakt faktor: 10.9, rok: 2022
    Způsob publikování: Omezený přístup
    https://www.sciencedirect.com/science/article/pii/S0008622322000768?via%3Dihub

    Nano-indentation at temperatures up to 600 degrees C has been applied to the (0001) surface of highly oriented pyrolytic graphite using a spherical diamond tip (similar to 10 mu m diameter). Cross-sectional observations of the indentations by dark field scanning transmission electron microscopy show an increased tendency at high temperature for inelastic deformation by buckling of the graphite crystals with kink formation. (C) 2022 Elsevier Ltd. All rights reserved.