Characterization of radical-enhanced atomic layer deposition process based on microwave surface wave generated plasma

  1. 1.
    0552189 - FZÚ 2022 RIV US eng J - Článek v odborném periodiku
    Tvarog, Drahoslav - Olejníček, Jiří - Kratochvíl, Jiří - Kšírová, Petra - Poruba, A. - Hubička, Zdeněk - Čada, Martin
    Characterization of radical-enhanced atomic layer deposition process based on microwave surface wave generated plasma.
    Journal of Applied Physics. Roč. 130, č. 1 (2021), č. článku 013301. ISSN 0021-8979. E-ISSN 1089-7550
    Grant CEP: GA MŠMT LM2018110; GA MŠMT(CZ) EF16_019/0000760; GA TA ČR(CZ) TM01000039; GA TA ČR TF03000025
    Grant ostatní: OP VVV - SOLID21(XE) CZ.02.1.01/0.0/0.0/16_019/0000760
    Institucionální podpora: RVO:68378271
    Klíčová slova: microwave surfatron * low-temperature plasma * ALD * TiO2 * plasma diagnostics
    Obor OECD: Fluids and plasma physics (including surface physics)
    Impakt faktor: 2.877, rok: 2021
    Způsob publikování: Omezený přístup
    https://doi.org/10.1063/5.0046829

    A plasma-assisted atomic layer deposition system employing a microwave surfatron plasma was developed and characterized by spatially resolved Langmuir probe diagnostics and optical emission spectroscopy. The deposition process was applied on TiO2 thin films prepared on Si wafers. The surfatron is equipped with a small ring electrode serving as a source of weak radio frequency plasma helping with fast and reliable ignition of the discharge in molecular gas. Results evaluated in the pure argon plasma proved that the plasma potential and the plasma density are homogeneous in the radial direction, while a rapid decrease was observed in the axial direction. Adding up to 30% of nitrogen into the gas mixture led to less homogeneous plasma parameters in the radial direction together with the increase of the electron effective temperature. Optical emission spectra revealed many Ar I lines of neutral atoms with only a few Ar II ions’ lines.