Počet záznamů: 1
Temperature dependence of the Hall coefficient of sensitive layer materials considered for DEMO Hall sensors
- 1.0532354 - ÚFP 2021 RIV CH eng J - Článek v odborném periodiku
Entler, Slavomír - Ďuran, Ivan - Kovařík, Karel - Sládek, Petr - Grover, Ondřej - Vilémová, Monika - Najman, D. - Kohout, Michal - Šebek, Josef - Výborný, Karel - Šobáň, Zbyněk
Temperature dependence of the Hall coefficient of sensitive layer materials considered for DEMO Hall sensors.
Fusion Engineering and Design. Roč. 153, April (2020), č. článku 111454. ISSN 0920-3796. E-ISSN 1873-7196.
[14th International Symposium on Fusion Nuclear Technology. Budapešť, 22.09.2019-27.09.2019]
Grant CEP: GA MŠMT(CZ) 8D15001
GRANT EU: European Commission(XE) 633053 - EUROfusion
Institucionální podpora: RVO:61389021 ; RVO:68378271
Klíčová slova: demo * Hall coefficient * Hall sensors * Magnetic diagnostics * Temperature
Obor OECD: Fluids and plasma physics (including surface physics); Nuclear physics (FZU-D)
Impakt faktor: 1.453, rok: 2020
Způsob publikování: Omezený přístup
https://www.sciencedirect.com/science/article/pii/S0920379620300028?via%3Dihub
The Hall sensors as a part of the DEMO magnetic diagnostics will perform an absolute measurement of the steady-state magnetic field. However, the magnitude of the Hall coefficients generally depends on the temperature. The paper presents an evaluation of the temperature dependencies of the Hall coefficients of materials considered for the DEMO Hall sensors from room temperature up to 550 °C. The results show that tantalum or molybdenum sensors would be the best in terms of the low temperature dependence of their Hall coefficient. Bismuth and antimony offer a Hall coefficient several orders of magnitude higher than other considered materials, but strongly temperature-dependent, while usability of bismuth is limited by its melting temperature of 271.4 °C. The gold, copper and platinum sensors feature modest temperature dependence of their Hall coefficients which might result in the necessity of dedicated temperature monitoring of these sensors in order to achieve sufficient measurement accuracy, similarly to bismuth and antimony.