Thermal decomposition of a peroxopolytitanic acid cryogel: TA/MS study

  1. 1.
    0471994 - ÚACH 2017 RIV NL eng J - Článek v odborném periodiku
    Palkovská, Monika - Slovák, V. - Šubrt, Jan - Boháček, Jaroslav - Havlín, J.
    Thermal decomposition of a peroxopolytitanic acid cryogel: TA/MS study.
    Thermochimica Acta. Roč. 647, JAN (2017), s. 1-7. ISSN 0040-6031. E-ISSN 1872-762X
    Grant CEP: GA ČR(CZ) GA14-20744S
    Institucionální podpora: RVO:61388980
    Klíčová slova: TiO2 thin-films * peroxo-polytitanic acid * sol-gel process * photocatalytic activity * titanium dioxides
    Obor OECD: Inorganic and nuclear chemistry
    Impakt faktor: 2.189, rok: 2017

    Thermal decomposition of a peroxopolytitanic acid cryogel was followed by simultaneous thermal analysis (TG/DTA) coupled with mass spectrometer (MS) and infrared spectroscope (FTIR). During the decomposition, the evolution of H2O (either residual moisture or as product of dehydration reactions), NH3 (precipitating agent used in preparation), O-2 (decomposition of peroxogroups), SO2 (decomposition of residual sulfates), N-2 (freezing agent in preparation), N2O, NO, NO2 (products of NH3 oxidation) and CO2 (adsorbed from atmosphere) was sought for. It was determined, that the decomposition is a four step process. During the first step, water and carbon dioxide evolve. At around 300 degrees C both N2O and CO2 (m/z = 44) were detected, as confirmed by FTIR spectroscopy. At 430-450 degrees C (depending of heating rate) amorphous phase crystallizes into anatase.
    Trvalý link: http://hdl.handle.net/11104/0269356

     
    Název souboruStaženoVelikostKomentářVerzePřístup
    Thermal decomposition.pdf02.5 MBAutorský postprintpovolen
     
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.