- High cycle fatigue of nickel-based superalloy MAR-M 247 at high tempe…
Počet záznamů: 1  

High cycle fatigue of nickel-based superalloy MAR-M 247 at high temperatures

  1. 1.
    0435146 - ÚFM 2015 RIV NL eng C - Konferenční příspěvek (zahraniční konf.)
    Šmíd, Miroslav - Kunz, Ludvík - Hutař, Pavel - Hrbáček, K.
    High cycle fatigue of nickel-based superalloy MAR-M 247 at high temperatures.
    XVII International Colloquium on Mechanical Fatigue of Metals (ICMFM17). Amsterdam: Elsevier, 2014 - (Gulagliano, M.; Vergani, L.), s. 329-332. Procedia Engineering, 74. ISSN 1877-7058.
    [ICMFM 2014 International Colloquium on Mechanical Fatigue of Metals /17./. Verbania (IT), 25.06.2014-27.06.2014]
    Grant CEP: GA MPO FR-TI4/030; GA MŠMT(CZ) EE2.3.20.0214
    Institucionální podpora: RVO:68081723
    Klíčová slova: High cycle fatigue * Superalloy * MAR-M 247 * High temperature * Fracture surface * S-N curve
    Kód oboru RIV: JL - Únava materiálu a lomová mechanika
    DOI: https://doi.org/10.1016/j.proeng.2014.06.273

    The nickel-based superalloy MAR-M 247 was experimentally studied in the area of high-cycle fatigue at temperatures 650, 800 and 900 °C. The alloy, a cast polycrystalline material processed by hot isostatic pressing (HIP), was subjected to symmetrical cyclic loading. The fracture surfaces of specimens were studied by scanning electron microscopy from the perspective of the influence of temperature on the fatigue damage mechanism and fatigue crack initiation. The extent of Stage I of crystallographic fatigue crack propagation and non-crystallographic Stage II differs with various test temperatures. Fatigue crack initiation sites were predominantly shrinkage pores inherited from casting. The general description of governing mechanisms of the fatigue crack initiation and the crack propagation are proposed.