    Campbellova, A. - Klapetek, P. - Buršíková, V. - Valtr, M. - Buršík, Jiří
    Small-load nanoindentation experiments on metals.
    Surface and Interface Analysis. Roč. 42, č. 6-7 (2010), s. 766-769. ISSN 0142-2421. E-ISSN 1096-9918.
    [European Conference on Applications of Surface and Interface Analysis /13./. Antalya, 18.10.2010-23.10.2010]
    Institutional research plan: CEZ:AV0Z20410507
    Keywords : nanoindentation * FCC metals * pop-in
    Subject RIV: BM - Solid Matter Physics ; Magnetism
    Impact factor: 1.247, year: 2010

    The loading curve dependency and presence of ´pop-in´effects were studied for different materials and indentation methods specifically on metals with face-centered cubic(Ni)and tetragonal(Sn)crystalline structures. The nanoindentation experiments were performed on CSM UNHT(ultra nano hardness tester)instrument using a diamond Berkovich tip and on an atomic force microscope using a steel indentation cantilever.