Application of visco-elasto plastic model to human trabecular bone based on results from nanoindentation and verified by time lapse X-Ray microtomography

  1. 1.
    0360875 - UTAM-F 2012 RIV BE eng C - Konferenční příspěvek (zahraniční konf.)
    Zlámal, Petr - Jiroušek, Ondřej - Kytýř, Daniel - Němeček, J.
    Application of visco-elasto plastic model to human trabecular bone based on results from nanoindentation and verified by time lapse X-Ray microtomography.
    ISB 2011. Brussels: International Society of Biomechanics, 2011 - (Feipel, V.), s. 211-212. ISBN 9789090260198.
    [ISB 2011. Brusel (BE), 03.07.2011-07.07.2011]
    Grant CEP: GA ČR(CZ) GAP105/10/2305
    Výzkumný záměr: CEZ:AV0Z20710524
    Klíčová slova: trabecular bone * nanoindentation * visco-elasto-plastic model
    Kód oboru RIV: FI - Traumatologie, ortopedie

    This paper deals with development of a numerical visco-elasto plastic material model for a single human trabeculae and its application on a complex sample. The elastic constants for this model were obtained directly from nanoindentation, remaining ones were determined indirectly from Finite Element Analysis (FEA). Identified material model was used for a Finite Element (FE) model of complex cylindrical sample of human trabecular bone. The geometry of the FE model was obtained from X-ray micro Computed Tomography. To verify the ability of the material model to describe deformation behavior of trabecular bone a cylindrical sample was incrementally loaded in compression and the deformed microstructure repetitively scanned.