    0583070 - ÚPT 2025 RIV US eng J - Journal Article
    Ronoh, K. - Novotný, Jan - Mrňa, Libor - Knápek, Alexandr - Sobola, Dinara
    Analysis of processing efficiency, surface, and bulk chemistry, and nanomechanical properties of the Monel® alloy 400 after ultrashort pulsed laser ablation.
    Materials Research Express. Roč. 11, č. 1 (2024), č. článku 016514. E-ISSN 2053-1591
    Institutional support: RVO:68081731 ; RVO:68081723
    Keywords : laser ablation * ablation efficiency * EDX * XPS * nanoindentation * Monel (R) alloy 400
    Impact factor: 2.3, year: 2022
    Method of publishing: Open access
    https://iopscience.iop.org/article/10.1088/2053-1591/ad184b
    Permanent Link: https://hdl.handle.net/11104/0351074
     
     
  2. 2.
    0582943 - ÚOCHB 2025 RIV NL eng J - Journal Article
    Thakur, G. C. N. - Uday, A. - Cebecauer, M. - Roos, W. H. - Cwiklik, Lukasz - Hof, M. - Jurkiewicz, P. - Melcrová, A.
    Charge of a transmembrane peptide alters its interaction with lipid membranes.
    Colloids and Surfaces B-Biointerfaces. Roč. 235, March (2024), č. článku 113765. ISSN 0927-7765. E-ISSN 1873-4367
    R&D Projects: GA ČR(CZ) GX19-26854X
    Institutional support: RVO:61388963
    Keywords : Integral membrane protein * FRET-GP * AFM imaging * AFM nanoindentation * MD simulation
    Impact factor: 5.8, year: 2022
    Method of publishing: Open access
    https://doi.org/10.1016/j.colsurfb.2024.113765
    Permanent Link: https://hdl.handle.net/11104/0350989
     
     
  3. 3.
    0579663 - FZÚ 2024 RIV PL eng C - Conference Paper (international conference)
    Kovář, J. - Fuis, V. - Čtvrtlík, Radim - Tomáštík, Jan
    The influence of tilt on Berkovich indentation of a steel sample using FEM analysis and nanoindentation.
    Proceedings of the conference Local Mechanical Properties. Warszawa: de Gruyter, 2022 - (Hvizdoš, P.; Shepa, I.; Ondrejová, K.; Bureš, R.; Martin, T.), s. 53-61. E-ISSN 1339-4533.
    [International Conference on Local Mechanical Properties /15./. Košice (SK), 11.05.2022-13.05.2022]
    R&D Projects: GA TA ČR TN01000038
    Research Infrastructure: e-INFRA CZ - 90140
    Institutional support: RVO:68378271
    Keywords : nanoindentation * indenter shape deviations * indenter tilt * indenter bluntness
    OECD category: Materials engineering
    https://sciendo.com/article/10.2478/pmp-2022-0007
    Permanent Link: https://hdl.handle.net/11104/0348475
     
     
  4. 4.
    0579525 - FZÚ 2024 RIV DE eng C - Conference Paper (international conference)
    Chmelíčková, Hana - Havelková, Martina - Hrubantová Písařiková, Aneta - Jílek, Vlastimil - Václavek, Lukáš
    Parameters optimization of Ti6Al4V alloy welding by pulsed Nd:YAG laser.
    Lasers in Manufacturing Conference 2023 - Proceedings. Mnichov: WLT, 2023, č. článku 149..
    [Lasers in Manufacturing Conference (LiM 2023). Online (DE), 26.06.2023-29.06.2023]
    R&D Projects: GA MŠMT LM2023032
    Institutional support: RVO:68378271
    Keywords : laser welding * Ti6Al4V * FEM model * nanoindentation * XRD analysis
    OECD category: Materials engineering
    Permanent Link: https://hdl.handle.net/11104/0348479
     
     
  5. 5.
    0578756 - ÚT 2024 CZ eng C - Conference Paper (international conference)
    Fiala, L. - Ballo, I. - Kovář, J. - Fuis, Vladimír
    Comparison of finite element simulation of tungsten nanoindentation with Berkovich and conical indenter.
    Engineering Mechanics 2023. Prague: Institute of Thermomechanics of the Czech Academy of Sciences, 2023 - (Radolf, V.; Zolotarev, I.), 63 - 66, s. 63-66. ISBN 978-80-87012-84-0. ISSN 1805-8248. E-ISSN 1805-8256.
    [Engineering Mechanics 2023 /29./. Milovy (CZ), 09.05.2023-11.05.2023]
    Institutional support: RVO:61388998
    Keywords : nanoindentation * FEM * Berkovich indenter * conical indenter * tungsten
    OECD category: Mechanical engineering
    https://www.engmech.cz/im/proceedings/search/2023
    Permanent Link: https://hdl.handle.net/11104/0351905
     
     
  6. 6.
    0565690 - ÚFP 2023 RIV US eng J - Journal Article
    Rohan, P. - Lukáč, František - Kolaříková, M. - Krum, S. - Horník, J. - Lukeš, J. - Šepitka, J. - Kuchař, J.
    Pulsed Plasma Surfacing of Titanium Matrix Cermet Based on B4C.
    Journal of Thermal Spray Technology. Roč. 31, č. 6 (2022), s. 1975-1984. ISSN 1059-9630. E-ISSN 1544-1016
    Institutional support: RVO:61389021
    Keywords : cermets processing * microstructure properties * nanoindentation testing * PTAW processing * Ti-6Al-4V feedstock * wear-resistant coatings applications
    OECD category: Materials engineering
    Impact factor: 3.1, year: 2022
    Method of publishing: Limited access
    https://link.springer.com/article/10.1007/s11666-022-01421-0
    Permanent Link: https://hdl.handle.net/11104/0337199
     
     
  7. 7.
    0565030 - ÚT 2023 RIV US eng J - Journal Article
    Kovář, J. - Fuis, Vladimír - Čtvrtlík, Radim - Tomáštík, Jan
    The discrepancy between the indentation curves obtained by the finite element method calculation with a Berkovich and a conical indenter.
    Journal of Materials Research. Roč. 37, č. 10 (2022), s. 1750-1761. ISSN 0884-2914. E-ISSN 2044-5326
    R&D Projects: GA TA ČR TN01000038
    Institutional support: RVO:61388998 ; RVO:68378271
    Keywords : nanoindentation * computing * elastic properties * fused silica * Ni
    OECD category: Applied mechanics; Materials engineering (FZU-D)
    Impact factor: 2.7, year: 2022
    Method of publishing: Limited access
    https://link.springer.com/article/10.1557/s43578-022-00574-6
    Permanent Link: https://hdl.handle.net/11104/0337616
     
     
  8. 8.
    0561614 - ÚFM 2023 RIV CH eng J - Journal Article
    Tinoco Navaro, Hector Andres - Fintová, Stanislava - Heikkila, I. - Herrero, D. - Vuoristo, T. - Dlouhý, Ivo - Hutař, Pavel
    Experimental and numerical study of micromechanical damage induced by MnS-based inclusions.
    Materials Science and Engineering A Structural Materials Properties Microstructure and Processing. Roč. 856, OCT (2022), č. článku 144009. ISSN 0921-5093. E-ISSN 1873-4936
    EU Projects: European Commission(XE) 747266 - RFCS-02-2016
    Program: INNOFAT
    Institutional support: RVO:68081723
    Keywords : Inclusions * MnS * Microtensile tests * Fatigue * Finite element analysis * Nanoindentation
    OECD category: Materials engineering
    Impact factor: 6.4, year: 2022
    Method of publishing: Limited access
    https://www.sciencedirect.com/science/article/pii/S0921509322013880?via%3Dihub
    Permanent Link: https://hdl.handle.net/11104/0334353
     
     
  9. 9.
    0560811 - FZÚ 2023 RIV CZ eng C - Conference Paper (international conference)
    Čech, J. - Haušild, P. - Karlík, M. - Nová, K. - Průša, F. - Novák, P. - Kopeček, Jaromír
    Fracture behavior of FeAlSi intermetallics.
    Acta Polytechnica CTU Proceedings. Prague: CTU, 2020 - (Nemecek, J.; Haušild, P.; Čtvrtlík, R.), s. 6-12. ISBN 978-80-01-06735-2. ISSN 2336-5382.
    [14th International Conference on Local Mechanical Properties. Praha (CZ), 06.11.2019-08.11.2019]
    R&D Projects: GA ČR(CZ) GA17-07559S
    Institutional support: RVO:68378271
    Keywords : FeAlSi * fracture toughness * nanoindentation * SPS
    OECD category: Condensed matter physics (including formerly solid state physics, supercond.)
    https://ojs.cvut.cz/ojs/index.php/APP/article/view/6660/5718
    Permanent Link: https://hdl.handle.net/11104/0333593
     
     
  10. 10.
    0557264 - ÚPT 2023 RIV CH eng J - Journal Article
    Plichta, Tomáš - Zahradníček, R. - Čech, V.
    Surface topography affects the nanoindentation data.
    Thin Solid Films. Roč. 745, 1 March (2022), č. článku 139105. ISSN 0040-6090. E-ISSN 1879-2731
    Research Infrastructure: CzechNanoLab - 90110
    Institutional support: RVO:68081731
    Keywords : Thin film * Plasma-enhanced chemical vapour deposition * Surface topography * Nanoindentation * Mechanical properties * Modulus of elasticity * Hardness * Atomic force microscopy
    OECD category: Coating and films
    Impact factor: 2.1, year: 2022
    Method of publishing: Limited access
    https://www.sciencedirect.com/science/article/pii/S0040609022000268