- 1.0465507 - ÚFM 2017 RIV GB eng J - Journal Article
Guth, S. - Petráš, Roman - Škorík, Viktor - Kruml, Tomáš - Man, Jiří - Lang, K. H. - Polák, Jaroslav
Influence of dwell times on the thermomechanical fatigue behavior of a directionally solidified Ni-base superalloy.
International Journal of Fatigue. Roč. 80, NOV (2015), s. 426-433. ISSN 0142-1123. E-ISSN 1879-3452
R&D Projects: GA MŠMT(CZ) EE2.3.30.0063
Institutional support: RVO:68081723
Keywords : Nickel base superalloy * Thermomechanical fatigue * Dwell time * Lifetime behavior * Damage mechanisms
Subject RIV: JL - Materials Fatigue, Friction Mechanics
Impact factor: 2.162, year: 2015
Permanent Link: http://hdl.handle.net/11104/0264075 - 2.0435373 - ÚFM 2015 RIV CH eng C - Conference Paper (international conference)
Jech, D. - Čelko, L. - Juliš, M. - Klakurková, L. - Slámečka, K. - Obrtlík, Karel - Švejcar, J.
Critical weak Points of Atmospheric Plasma Sprayed Thermal Barrier Coatings.
Metallography XV. Zurich: Trans Tech Publications, 2014 - (Longauerová, M.; Zubko, P.), s. 567-572. Materials Science Forum, 782. ISBN 978-3-03835-072-9. ISSN 0255-5476.
[Metallography2013 - International Symposium on Metalography /15./. Stará Lesná (SK), 24.04.2013-26.04.2013]
R&D Projects: GA ČR(CZ) GAP107/11/2065; GA MŠMT(CZ) ED1.1.00/02.0068
Institutional support: RVO:68081723
Keywords : Thermal barrier coating * Thermally grown oxide * nickel base superalloy
Subject RIV: JK - Corrosion ; Surface Treatment of Materials
Permanent Link: http://hdl.handle.net/11104/0239444 - 3.0435364 - ÚFM 2015 RIV CH eng C - Conference Paper (international conference)
Čelko, L. - Hutařová, S. - Petrenec, M. - Obrtlík, Karel - Hrčková, M. - Podrábský, T.
Microstructural Characterization of Slurry Aluminide Diffusion Coatings.
Metallography XV. Zurich: Trans Tech Publications, 2014 - (Longauerová, M.; Zubko, P.), s. 584-589. Materials Science Forum, 782. ISBN 978-3-03835-072-9. ISSN 0255-5476.
[Metallography2013 - International Symposium on Metalography /15./. Stará Lesná (SK), 24.04.2013-26.04.2013]
R&D Projects: GA ČR(CZ) GAP107/11/2065; GA MŠMT(CZ) ED1.1.00/02.0068
Institutional support: RVO:68081723
Keywords : nickel aluminides * diffusion coating * nickel base superalloy
Subject RIV: JK - Corrosion ; Surface Treatment of Materials
Permanent Link: http://hdl.handle.net/11104/0239481 - 4.0435156 - ÚFM 2015 RIV CH eng C - Conference Paper (international conference)
Šmíd, Miroslav - Obrtlík, Karel
Surface relief evolution in IN792-5A nickel superalloy under high temperature fatigue straining with hold times.
Materials Structure and Micromechanics of Fracture VII. Zurich: Trans Tech Publications, 2014 - (Šandera, P.), s. 429-432. Key Engineering Materials, 592-593. ISBN 978-3-03785-934-6. ISSN 1013-9826.
[MSMF 7 - International Conference on Materials Structure & Micromechanics of Fracture /7./. Brno (CZ), 01.07.2013-03.07.2013]
R&D Projects: GA MPO FR-TI3/055; GA ČR(CZ) GAP107/11/2065; GA MŠMT(CZ) EE2.3.20.0214
Institutional support: RVO:68081723
Keywords : Nickel-base superalloy * Surface relief * Fatigue * Hold times * High temperature fatigue
Subject RIV: JL - Materials Fatigue, Friction Mechanics
Permanent Link: http://hdl.handle.net/11104/0239055 - 5.0421225 - ÚFM 2014 RIV DE eng C - Conference Paper (international conference)
Šmíd, Miroslav - Obrtlík, Karel - Polák, Jaroslav
Dwell effect on low cycle fatigue behaviour of cast superalloy Inconel 792-5A at 800 °C.
Proceedings of the Seventh International Conference on Low Cycle Fatigue - LCF7. Berlín: DMV, 2013, s. 113-118. ISBN 978-3-9814516-2-7.
[LCF7 - International Conference on Low Cycle Fatigue /7./. Aachen (DE), 09.09.2013-11.09.2013]
R&D Projects: GA ČR(CZ) GAP204/11/1453; GA ČR(CZ) GAP107/11/2065; GA MPO FR-TI4/030
Institutional support: RVO:68081723
Keywords : nickel base superalloy * low cycle fatigue * dwell * high temperature fatigue * surface relief * dislocation structure
Subject RIV: JL - Materials Fatigue, Friction Mechanics
Permanent Link: http://hdl.handle.net/11104/0228182