- 1.0579198 - ÚFM 2025 RIV US eng J - Journal Article
Gamanov, Štěpán - Dlouhý, Antonín - Bürger, D. - Eggeler, G. - Thome, P.
Evolution of local misorientations in the γ/γ'-microstructure of single crystal superalloys during creep studied with the rotation vector baseline (RVB) EBSD method.
Microscopy Research and Technique. Roč. 87, č. 3 (2024), s. 516-533. ISSN 1059-910X. E-ISSN 1097-0029
Institutional support: RVO:68081723
Keywords : interfacial dislocation networks * temperature * deformation * misfit * stress * local dislocation densities * misorientations between gamma and gamma' phases * rotation vector baseline EBSD method * scanning transmission electron microscopy * single crystal Ni-base superalloys
OECD category: Materials engineering
Impact factor: 2.5, year: 2022
Method of publishing: Open access
https://analyticalsciencejournals.onlinelibrary.wiley.com/doi/10.1002/jemt.24453
Permanent Link: https://hdl.handle.net/11104/0352715 - 2.0534080 - ÚFM 2021 RIV CH eng J - Journal Article
Bürger, D. - Dlouhý, Antonín - Yoshimi, K. - Eggeler, G.
How Nanoscale Dislocation Reactions Govern Low- Temperature and High-Stress Creep of Ni-Base Single Crystal Superalloys.
Crystals. Roč. 10, č. 2 (2020), č. článku 134. ISSN 2073-4352. E-ISSN 2073-4352
Institutional support: RVO:68081723
Keywords : electron-microscopy * planar defects * precipitation * mechanisms * anisotropy * phase * shear * microstructure * deformation * faults * dislocation reactions * single crystal Ni-base superalloys * shear creep testing * transmission electron microscopy * nucleation of planar fault ribbons
OECD category: Materials engineering
Impact factor: 2.589, year: 2020
Method of publishing: Open access
https://www.mdpi.com/2073-4352/10/2/134
Permanent Link: http://hdl.handle.net/11104/0312299 - 3.0464792 - ÚFM 2017 RIV GB eng J - Journal Article
WU, X. - Wollgramm, P. - Somsen, C. - Dlouhý, Antonín - Kostka, A. - Eggeler, G.
Double minimum creep of single crystal Ni-base superalloys.
Acta Materialia. Roč. 112, JUN (2016), s. 242-260. ISSN 1359-6454. E-ISSN 1873-2453
R&D Projects: GA ČR(CZ) GA14-22834S
Institutional support: RVO:68081723
Keywords : Single crystal Ni-base superalloys * Primary creep * Transmission electron microscopy * Dislocations * Stacking faults
Subject RIV: JG - Metallurgy
Impact factor: 5.301, year: 2016
Permanent Link: http://hdl.handle.net/11104/0263576 - 4.0387739 - ÚFM 2013 RIV NL eng J - Journal Article
Agudo Jácome, L. - Eggeler, G. - Dlouhý, Antonín
Advanced scanning transmission stereo electron microscopy of structural and functional engineering materials.
Ultramicroscopy. Roč. 122, NOV (2012), s. 48-59. ISSN 0304-3991. E-ISSN 1879-2723
R&D Projects: GA ČR GA202/09/2073
Institutional research plan: CEZ:AV0Z20410507
Keywords : stereoscopy * scanning transmission electron microscopy * single crystal Ni-base superalloys * Dislocation substructures * Foil thickness measurement
Subject RIV: BM - Solid Matter Physics ; Magnetism
Impact factor: 2.470, year: 2012
Permanent Link: http://hdl.handle.net/11104/0216832