Number of the records: 1
Wolframové cermety s karbidem zirkonia a hafnia
- 1.
SYSNO ASEP 0350185 Document Type C - Proceedings Paper (int. conf.) R&D Document Type Conference Paper Title Wolframové cermety s karbidem zirkonia a hafnia Title Tungsten cermets with zirconium and hafnium carbides Author(s) Brožek, Vlastimil (UFP-V) RID
Ctibor, Pavel (UFP-V) RID, ORCID
Matušek, M. (CZ)
Sedláček, J. (CZ)Source Title Metal 2010 - 19th international conference on metallurgy and materials. - Ostrava : Tanger s.r.o, 2010 - ISBN 978-80-87294-15-4 Pages s. 112-117 Number of pages 6 s. Publication form CD-ROM - CD-ROM Action International Conference on Metallurgy and Materials METAL 2010 /19th./ Event date 18.05.2010-20.05.2010 VEvent location Rožnov pod Radhoštěm Country CZ - Czech Republic Event type WRD Language cze - Czech Country CZ - Czech Republic Keywords plasma spraying ; cermets ; tungsten ; zirconium carbide ; hafnium carbide Subject RIV CA - Inorganic Chemistry CEZ AV0Z20430508 - UFP-V (2005-2011) Annotation Cermety s wolframovou matricí a funkčními složkami ZrC a HfC s absolutně nejvyššími body tání představují materiál s extrémně vysokými užitnými vlastnostmi za vysokých teplot. Wolframové cermety s obsahem 10, 20 a 30 % funkční složky byly připraveny dvěma rozdílnými postupy a porovnány jejich vlastnosti. První serie byla připravena postupem práškové metalurgie. Zhomogenizovaná a předlisovaná směs prášků byla slinována při teplotě 2000°C a tlaku 6 GPa v aparatuře typu BELT. Druhá serie byla připravena metodou plasma spraying dvěma odlišnými postupy. V prvním případě byly do proudu vodou stabilizovaného plazmatu, produkovaného generátorem WSP®, vnášeny samostatnými podavači prášky W a ZrC nebo W a HfC. Vzdálenost podavačů od výstupní trysky plazmatu od 25 do 75 mm byla ovlivněna rozdílnými kinetickými parametry prášků s rozdílnou granulometrií a hustotou. Druhý postup spočíval v depozici sferoidizovaných práškových směsí, připravených metodou spray-drying s obsahem 5%pojiva Description in English Cermets with tungsten matrix and functional components of ZrC and HfC with absolutely highest meeting points are materials with good properties at high temperature exposure. Tungsten based cermets with 10, 20 and 30 % of the functional component were prepared by two different procedures and their properties were compared. The first series of the samples was manufactured by powder metallurgy. A homogenized and preformed mixture of powders was sintered at 2000°C and pressure 6 GPa by hot-pressing technique in the apparatus of BELT-type. The second series was prepared by plasma spraying with water-stabilized plasma WSP® by two different procedures. In the first case the powders of W and ZrC (or W and HfC) were injected into the plasma jet by two separate feeders. The feeding distance 25 to 75 mm was affected by different kinetic parameters, different size distribution and density. The second case represents deposition of pre-spheroidized powder mixtures prepared by spray drying Workplace Institute of Plasma Physics Contact Vladimíra Kebza, kebza@ipp.cas.cz, Tel.: 266 052 975 Year of Publishing 2011
Number of the records: 1