Slow pyrolysis of waste polyethylene terephthalate yielding paraldehyde, ethylene glycol, benzoic acid and clean fuel

  1. SYS0556401
    005
      
    20240103230620.6
    014
      
    $a 85126542413 $2 SCOPUS
    014
      
    $a 000772950400009 $2 WOS
    017
    70
    $a 10.1016/j.polymdegradstab.2022.109900 $2 DOI
    101
    0-
    $a eng
    102
      
    $a GB
    200
    1-
    $a Slow pyrolysis of waste polyethylene terephthalate yielding paraldehyde, ethylene glycol, benzoic acid and clean fuel
    215
      
    $a 9 s. $c E
    463
    -1
    $1 001 cav_un_epca*0257484 $1 011 $a 0141-3910 $e 1873-2321 $1 200 1 $a Polymer Degradation and Stability $v Roč. 198, APR 2022 (2022) $1 210 $c Elsevier
    608
      
    $a Article
    610
      
    $a Pyrolysis
    610
      
    $a Waste PET
    610
      
    $a Paraldehyde
    610
      
    $a Ethylene glycol
    610
      
    $a Benzoic acid
    610
      
    $a Clean fuel
    700
    -1
    $3 cav_un_auth*0102487 $a Straka $b Pavel $p USMH-B $i Odd. struktury a vlastností materiálů $j Department of Materials Structure and Properties $T Ústav struktury a mechaniky hornin AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0259944 $a Bičáková $b Olga $p USMH-B $i Odd. struktury a vlastností materiálů $j Department of Materials Structure and Properties $y CZ $T Ústav struktury a mechaniky hornin AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0258084 $a Šupová $b Monika $p USMH-B $i Odd. kompozitních a uhlíkových materiálů $j Department of Composites and Carbon Material $y CZ $T Ústav struktury a mechaniky hornin AV ČR, v. v. i.
    856
      
    $u https://www.sciencedirect.com/science/article/pii/S0141391022000866?via%3Dihub $9 RIV