Semi-automatic spray pyrolysis deposition of thin, transparent, titania films as blocking layers for dye-sensitized and perovskite solar cells

  1. 1.
    0488906 - ÚFCH JH 2019 RIV DE eng J - Journal Article
    Krýsová, Hana - Krýsa, J. - Kavan, Ladislav
    Semi-automatic spray pyrolysis deposition of thin, transparent, titania films as blocking layers for dye-sensitized and perovskite solar cells.
    Beilstein Journal of Nanotechnology. Roč. 9, APR 2018 (2018), s. 1135-1145. ISSN 2190-4286. E-ISSN 2190-4286
    R&D Projects: GA ČR GA17-20008S; GA ČR(CZ) GA18-08959s; GA MŠMT(CZ) EF16_013/0001821
    Institutional support: RVO:61388955
    Keywords : blocking films * FTO * solar cells
    OECD category: Electrochemistry (dry cells, batteries, fuel cells, corrosion metals, electrolysis)
    Impact factor: 2.269, year: 2018
    Method of publishing: Open access

    For proper function of the negative electrode of dye-sensitized and perovskite solar cells, the deposition of a nonporous blocking film is required on the surface of F-doped SnO2 (FTO) glass substrates. Such a blocking film can minimise undesirable parasitic processes, for example, the back reaction of photoinjected electrons with the oxidized form of the redox mediator or with the hole-transporting medium can be avoided. In the present work, thin, transparent, blocking TiO2 films are prepared by semi-automatic spray pyrolysis of precursors consisting of titanium diisopropoxide bis(acetylacetonate) as the main component. The variation in the layer thickness of the sprayed films is achieved by varying the number of spray cycles. The parameters investigated in this work were deposition temperature (150, 300 and 450 °C), number of spray cycles (20–200), precursor composition (with/without deliberately added acetylacetone), concentration (0.05 and 0.2 M) and subsequent post-calcination at 500 °C. The photo-electrochemical properties were evaluated in aqueous electrolyte solution under UV irradiation. The blocking properties were tested by cyclic voltammetry with a model redox probe with a simple one-electron-transfer reaction. Semi-automatic spraying resulted in the formation of transparent, homogeneous, TiO2 films, and the technique allows for easy upscaling to large electrode areas. The deposition temperature of 450 °C was necessary for the fabrication of highly photoactive TiO2 films. The blocking properties of the as-deposited TiO2 films (at 450 °C) were impaired by post-calcination at 500 °C, but this problem could be addressed by increasing the number of spray cycles. The modification of the precursor by adding acetylacetone resulted in the fabrication of TiO2 films exhibiting perfect blocking properties that were not influenced by post-calcination. These results will surely find use in the fabrication of large-scale dye-sensitized and perovskite solar cells.
    Permanent Link: http://hdl.handle.net/11104/0283419

     
    FileDownloadSizeCommentaryVersionAccess
    0488906.pdf14.8 MBopen accessPublisher’s postprintopen-access
     
Number of the records: 1  

  This site uses cookies to make them easier to browse. Learn more about how we use cookies.