Number of the records: 1  

Thermomechanical and isothermal fatigue properties of MAR-M247 superalloy

  1. 1.
    0585632 - ÚFM 2025 RIV NL eng J - Journal Article
    Šulák, Ivo - Obrtlík, Karel
    Thermomechanical and isothermal fatigue properties of MAR-M247 superalloy.
    Theoretical and Applied Fracture Mechanics. Roč. 131, Jun (2024), č. článku 104443. ISSN 0167-8442. E-ISSN 1872-7638
    Institutional support: RVO:68081723
    Keywords : Thermomechanical fatigue * Nickel-based superalloy * Damage mechanisms * Lifetime prediction model
    OECD category: Materials engineering
    Impact factor: 5.3, year: 2022
    Method of publishing: Limited access
    https://www.sciencedirect.com/science/article/pii/S0167844224001927?via%3Dihub

    Thermomechanical low-cycle fatigue (TMF) tests were performed on polycrystalline cast nickel-based superalloy
    MAR-M247 under in-phase (IP) and out-of phase (OP) loading in the temperature range of 500–900 ◦C. A
    constant heating and cooling rate of 5 ◦C.s− 1 was selected. Furthermore, isothermal low-cycle fatigue (ILCF) tests
    with the same cycle period as TMF cycle were carried out at the maximal temperature of TMF cycle (900 ◦C). All
    tests ran under strain control and fully reversed cycle on solid cylindrical specimens in laboratory air. High
    resolution scanning electron microscopy and transmission electron microscopy were utilized to characterize the
    damage mechanism occurring during TMF and ILCF loading. The cyclic deformation and lifetime behaviour as
    well as damage mechanisms dependent on loading regime were examined. Results show that the TMF loading
    has a detrimental effect on the lifetime of MAR-M247. Lifetime reduction is most significant under IP loading.
    The fracture surfaces are characterized by typical striation fields, where the largest spacing between striations
    was observed for IP loading with prevailing intercrystalline cracking followed by OP and isothermal ILCF loading
    with transcrystalline crack propagation. To improve discussion of obtained results, experimental data were
    compared with damage and life prediction models.
    Permanent Link: https://hdl.handle.net/11104/0353317

     
     