    Small scale tests of cement with focused ion beam and nanoindentation.
    MATEC Web of Conferences. Vol. 310. Paris: EDP Sciences, 2020, č. článku 00053. E-ISSN 2261-236X.
    [International scientific conference structural and physical aspects of construction engineering (SPACE 2019) /4./. Štrbské pleso (SK), 13.11.2019-15.11.2019]
    R&D Projects: GA ČR(CZ) GA17-05360S
    Institutional support: RVO:68378271
    Keywords : cement * focused ion beam * finits element method
    OECD category: Condensed matter physics (including formerly solid state physics, supercond.)
    https://www.matec-conferences.org/articles/matecconf/pdf/2020/06/matecconf_space20_00053.pdf

    The effect of heat on the microstructure of cement during different FIB energy loads in studied. Micrometer sized beams were bent to reveal strength and fracture characteristics.