Characterization of NiTi alloys by instrumented nanoindentation: experiments and simulations

  1. 1.
    0445091 - ÚT 2016 GB eng A - Abstract
    Frost, Miroslav - Kruisová, Alena - Sháněl, Vít - Sedlák, Petr - Haušild, P. - Kabla, M. - Shilo, D. - Landa, Michal
    Characterization of NiTi alloys by instrumented nanoindentation: experiments and simulations.
    The International Conference on Shape Memory and Superelastic Technologies. Enston, Velká Británie: ASM International, 2015. s. 68-68.
    [Conference on Shape Memory and Superelastic Technologies (SMST 2015). 18.05.2015-22.05.2015, Enston]
    R&D Projects: GA ČR(CZ) GP14-28306P
    Grant - others:Rada Programu interní podpory projektů mezinárodní spolupráce AV ČR(CZ) M100761203
    Program: M
    Institutional support: RVO:61388998
    Keywords : numerical simulations * nanoindentation * shape memory alloys
    Subject RIV: BM - Solid Matter Physics ; Magnetism
    http://www.asminternational.org/conferences/resources/conference-proceedings/-/journal_content/56/10192/25094836/PUBLICATION

    This study aims to verify applicability of the recently developed constitutive model for NiTi-based SMA in simulations of nanoindentation tests. The model is fitted to a particular sample material using experimental data and a series of simulations mimicking tests at various temperatures are performed.