Cyclic plastic response of nickel-based superalloys at room and at elevated temperatures

  1. 1.
    0399434 - ÚFM 2014 RIV DE eng C - Conference Paper (international conference)
    Polák, Jaroslav - Petrenec, Martin - Chlupová, Alice - Tobiáš, Jiří - Petráš, Roman
    Cyclic plastic response of nickel-based superalloys at room and at elevated temperatures.
    Proceedings of the Seventh International Conference on Low Cycle Fatigue - LCF7. Berlín: DMV, 2013, s. 107-112. ISBN 978-3-9814516-2-7.
    [LCF7 - International Conference on Low Cycle Fatigue /7./. Aachen (DE), 09.09.2013-11.09.2013]
    R&D Projects: GA ČR(CZ) GAP204/11/1453
    Institutional support: RVO:68081723
    Keywords : superalloys * elevated temperature * hysteresis loop
    Subject RIV: JL - Materials Fatigue, Friction Mechanics

    Nickel-based IN 738LC superalloy has been cycled at increasing strain amplitudes at room temperature and at 800 °C. Hysteresis loops were analyzed using statistical theory of the hysteresis loop and dislocation structure of specimens cycled at these two temperatures were studied. The analysis of the loop shapes yields effective stresses of the matrix and of the precipitates and the probability density function of the critical internal stresses at both temperatures. It allows disclosing the sources of the high cyclic stress.