The use of atomic force microscopy for the surface analysis of complex polymer materials
- 1.0377737 - ÚMCH 2013 FR eng A - Abstract
Poreba, Rafal - Špírková, Milena
The use of atomic force microscopy for the surface analysis of complex polymer materials.
Abstract book. Ecully: Ecole Centrale de Lyon, 2012. s. 221-222.
[International Conference on Surface Modification Technologies /26./ - SMT 26. 20.06.2012-22.06.2012, Ecully]
R&D Projects: GA ČR GAP108/10/0195; GA AV ČR(CZ) IAAX08240901
Grant - others:AV ČR(CZ) M200500903
Institutional research plan: CEZ:AV0Z40500505
Institutional support: RVO:61389013
Keywords : atomic force microscopy * organic-inorganic nanocomposite * nanostructured polyurethane