Shape of gamma prime precipitates in single crystal superalloy SC16 studied by SANS

  1. 1.
    0183749 - UJF-V 960088 DE eng V - Research Report
    Wiedenmann, A. - Mukherji, D. - Wahi, R. - Lemke, J. - Strunz, Pavel
    Shape of gamma prime precipitates in single crystal superalloy SC16 studied by SANS.
    Berlin: Hahn Meitner Institut, 1996. 249-250 s. BENSC Experimental Reports 1995.
    R&D Projects: GA AV ČR IAA148404
    Permanent Link: http://hdl.handle.net/11104/0080213

     
     