Počet záznamů: 1
Non-isothermal kinetics of cold crystallization in multicomponent PLA/thermoplastic polyurethane/nanofiller system
- 1.
SYSNO ASEP 0480540 Druh ASEP J - Článek v odborném periodiku Zařazení RIV J - Článek v odborném periodiku Poddruh J Článek ve WOS Název Non-isothermal kinetics of cold crystallization in multicomponent PLA/thermoplastic polyurethane/nanofiller system Tvůrce(i) Kratochvíl, Jaroslav (UMCH-V) RID
Kelnar, Ivan (UMCH-V) RID, ORCIDZdroj.dok. Journal of Thermal Analysis and Calorimetry. - : Akadémiai Kiadó - ISSN 1388-6150
Roč. 130, č. 2 (2017), s. 1043-1052Poč.str. 10 s. Jazyk dok. eng - angličtina Země vyd. HU - Maďarsko Klíč. slova poly(lactic acid) ; cold crystallization ; thermoplastic polyurethane Vědní obor RIV JI - Kompozitní materiály Obor OECD Composites (including laminates, reinforced plastics, cermets, combined natural and synthetic fibre fabrics CEP GA16-03194S GA ČR - Grantová agentura ČR Institucionální podpora UMCH-V - RVO:61389013 UT WOS 000413264100046 EID SCOPUS 85019055420 DOI 10.1007/s10973-017-6417-y Anotace The effect of platy and tubular nanofillers (NF) in combination with thermoplastic polyurethane (TPU) on cold non-isothermal crystallization (NIC) of poly(lactic acid) (PLA) was studied by differential scanning calorimetry. The data were processed using a recently proposed method of evaluating NIC kinetics. The results indicate that the NF/TPU combination leads to crystallization behaviour of the PLA matrix which is dissimilar from that of the NF-free blend and neat PLA. Addition of organophilized montmorillonite (C30) results in a dual effect on PLA crystallinity—stimulation at lower concentrations and suppression at higher loadings. In the case of halloysite nanotubes (HNT), this effect is practically absent. Crystallinity of injection-moulded samples is significantly increased by cold NIC. This indicates a synergy originating in a complex effect of NF/TPU, e.g. NF-induced changes in morphology and interphase parameters supporting the solid annealing process. TPU partially eliminates negative effect of high NF contents on cold crystallization rate. This effect is more marked in the remelted samples where the rate increases for all NF loadings. This is probably caused by absence of as-prepared crystallites in combination with higher mobility of PLA chains due to presence of TPU. The observed differences between C30 and HNT could be attributed to differences in size, shape, and specific surface. The results indicate that synergistic and antagonistic effects of NF/polymeric modifiers on mechanical and other material parameters are also significantly determined by the effects on crystallization of the matrix. Pracoviště Ústav makromolekulární chemie Kontakt Eva Čechová, cechova@imc.cas.cz ; Tel.: 296 809 358 Rok sběru 2018
Počet záznamů: 1