Počet záznamů: 1  

Surface profile evolution and fatigue crack initiation in Sanicro 25 steel at room temperature

  1. SYS0465502
    LBL
      
    02591^^^^^2200409^^^450
    005
      
    20240103212945.1
    014
      
    $a 000372560800025 $2 WOS
    014
      
    $a 84957068456 $2 SCOPUS
    017
    70
    $a 10.1016/j.msea.2016.02.016 $2 DOI
    100
      
    $a 20161125d m y slo 03 ba
    101
    0-
    $a eng $d eng
    102
      
    $a CH
    200
    1-
    $a Surface profile evolution and fatigue crack initiation in Sanicro 25 steel at room temperature
    215
      
    $a 8 s.
    463
    -1
    $1 001 cav_un_epca*0257216 $1 011 $a 0921-5093 $e 1873-4936 $1 200 1 $a Materials Science and Engineering A Structural Materials Properties Microstructure and Processing $v Roč. 658, MAR (2016), s. 221-228 $1 210 $c Elsevier
    610
    0-
    $a Sanicro 25 steel
    610
    0-
    $a Fatigue crack initiation
    610
    0-
    $a Persistent slip markings
    610
    0-
    $a Extrusions
    610
    0-
    $a Intrusions
    700
    -1
    $3 cav_un_auth*0101313 $a Polák $b Jaroslav $i Nízkocyklová únava $j Low cycle fatigue $p UFM-A $w Low Cycle Fatigue Group $z A $4 070 $9 40 $T Ústav fyziky materiálů AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0287050 $a Petráš $b Roman $i Nízkocyklová únava $j Low cycle fatigue $p UFM-A $4 070 $9 30 $T Ústav fyziky materiálů AV ČR, v. v. i.
    701
    -1
    $3 cav_un_auth*0307434 $a Chai $b G. $y SE $4 070 $9 15
    701
    -1
    $3 cav_un_auth*0303976 $a Škorík $b Viktor $i Nízkocyklová únava $j Low cycle fatigue $p UFM-A $w Low Cycle Fatigue Group $y SK $z A $4 070 $9 15 $T Ústav fyziky materiálů AV ČR, v. v. i.
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.