Phase transformations and fatigue of NiTi

  1. 1.
    SYSNO ASEP0485660
    Druh ASEPC - Konferenční příspěvek (mezinárodní konf.)
    Zařazení RIVD - Článek ve sborníku
    NázevPhase transformations and fatigue of NiTi
    Tvůrce(i) Alarcon, E. (FR)
    Heller, Luděk (FZU-D) RID, ORCID
    Chirani, S.A. (FR)
    Šittner, Petr (FZU-D) RID, ORCID
    Saint-Sulpice, L. (FR)
    Calloch, S. (FR)
    Celkový počet autorů6
    Číslo článku03011
    Zdroj.dok.ESOMAT 2015 - 10th European Symposium on Martensitic Transformations. - P.A. de Courtabœuf : E D P Sciences, 2015 / Schryvers N. ; Van Humbeeck J. - ISSN 2261-236X - ISBN 978-2-7598-1925-6
    Rozsah strans. 1-6
    Poč.str.6 s.
    Forma vydáníOnline - E
    AkceEuropean Symposium on Martensitic Transformations /10./
    Datum konání14.09.2015 - 18.09.2015
    Místo konáníAntwerp
    ZeměBE - Belgie
    Typ akceWRD
    Jazyk dok.eng - angličtina
    Země vyd.FR - Francie
    Klíč. slovashape memory alloys ; nitinol ; martensitic transformation ; fatigue
    Vědní obor RIVJL - Únava materiálu a lomová mechanika
    Obor OECDAudio engineering, reliability analysis
    CEPGA14-15264S GA ČR - Grantová agentura ČR
    GAP107/12/0800 GA ČR - Grantová agentura ČR
    Institucionální podporaFZU-D - RVO:68378271
    UT WOS000372402800026
    EID SCOPUS84976508049
    DOI10.1051/matecconf/20153303011
    AnotaceTensile fatigue of superelastic medical graded NiTi wires was analysed in stress control regime with special attention paid to the deformation/transformation processes involved. Concave shaped samples were machined from NiTi wires allowing us to confine deformation processes into the centre of the sample. The localization of phase transformations within the centre was confirmed using in-situ infrared imaging. Characteristic stress-displacement responses for amplitudes inducing either R-phase only or both R-phase and martensite were identified for these samples. A limited number of pull-pull fatigue tests in force-control regime were performed. The obtained S-N curve and associated stress-displacement responses allowed for identification of three fatigue regimes differing in the fatigue life-time by orders of magnitude. Particularly, fatigue life-time deteriorating effect of R-phase transformation was identified.
    PracovištěFyzikální ústav
    KontaktKristina Potocká, potocka@fzu.cz, Tel.: 220 318 579
    Rok sběru2018
Počet záznamů: 1  

  Tyto stránky využívají soubory cookies, které usnadňují jejich prohlížení. Další informace o tom jak používáme cookies.